Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 80.0 - 110 µm/m-°C @Temperature 20.0 °C |
44.4 - 61.1 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
CTE, linear | 80.0 - 110 µm/m-°C @Temperature 20.0 °C |
44.4 - 61.1 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
CTE, linear | 90.0 - 110 µm/m-°C | 50.0 - 61.1 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
CTE, linear | 3.00 - 110 µm/m-°C | 1.67 - 61.1 µin/in-°F | Average value: 23.2 µm/m-°C Grade Count:47 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
CTE, linear | 30.0 - 110 µm/m-°C | 16.7 - 61.1 µin/in-°F | Average value: 68.9 µm/m-°C Grade Count:12 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
CTE, linear | 40.0 - 110 µm/m-°C | 22.2 - 61.1 µin/in-°F | Average value: 80.3 µm/m-°C Grade Count:13 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear | 28.8 - 110 µm/m-°C | 16.0 - 61.1 µin/in-°F | Average value: 85.4 µm/m-°C Grade Count:32 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
CTE, linear | 68.0 - 110 µm/m-°C | 37.8 - 61.1 µin/in-°F | Average value: 87.8 µm/m-°C Grade Count:28 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
CTE, linear | 50.0 - 110 µm/m-°C | 27.8 - 61.1 µin/in-°F | Average value: 68.2 µm/m-°C Grade Count:24 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
CTE, linear | 14.4 - 110 µm/m-°C | 8.00 - 61.1 µin/in-°F | Average value: 35.9 µm/m-°C Grade Count:53 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ASTM D696 |
Guarniflon PTFE G456 Polytetrafluoroethylene 25% Hard Carbon PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
CTE, linear | 75.0 - 110 µm/m-°C | 41.7 - 61.1 µin/in-°F | ASTM D696 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ISO 11359 |
Styrolution Luran® S 767KE ASA Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos.. |
|||
CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ISO 11359 |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ISO 11359 |
Styrolution Terluran® HI-12 ABS Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution |
|||
CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ISO 11359 |
Styrolution Terluran® GP-25 ABS Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se.. |
|||
CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ISO 11359 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
CTE, linear | 60.0 - 110 µm/m-°C | 33.3 - 61.1 µin/in-°F | Average value: 73.5 µm/m-°C Grade Count:20 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
CTE, linear | 21.6 - 110 µm/m-°C | 12.0 - 61.1 µin/in-°F | Average value: 66.6 µm/m-°C Grade Count:27 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |