Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 88.0 µm/m-°C @Temperature 20.0 °C |
48.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical NS-161 ABS, Antistatic, High Strength Information Provided by LG Chem |
|||
CTE, linear | 88.0 µm/m-°C | 48.9 µin/in-°F | ASTM D696 |
Eastman Tritan MP100 Copolyester Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co.. |
|||
CTE, linear | 88.0 µm/m-°C | 48.9 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® H20E-175 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-175 is a two component epoxy designed for semiconductor die-attach. It is a higher Tg version of EPO-TEK® H20E. It was designed to be used in semiconductor / J.. |
|||
CTE, linear | 88.0 µm/m-°C @Temperature 20.0 °C |
48.9 µin/in-°F @Temperature 68.0 °F |
modified; ASTM D696 |
LyondellBasell DEXFLEX® 711 TPO Description: DEXFLEX® 711 is a thermoplastic olefinic elastomer compounded with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color matched.. |
|||
CTE, linear | 88.0 - 104 µm/m-°C | 48.9 - 57.8 µin/in-°F | Average value: 94.0 µm/m-°C Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |