Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 80.6 µm/m-°C | 44.8 µin/in-°F | 90 Minute UV Cure + Thermal; T<Tg; ASTM E831-93 |
3D Systems Accura® SI 40 Plastic for the SLA® 500 System Accura 40 "Ar" or "Hc" type materials - for the SLA 500 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |