Polymer Property : CTE, linear = 44.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 79.2 µm/m-°C

@Temperature 20.0 °C
44.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Network Polymers Kepital® TC30-20
Description: Natural Acetal Copolymer, 10% Talc Reinforced GradeInformation provided by Network Polymers Inc.
CTE, linear 79.2 µm/m-°C

@Temperature 20.0 °C
44.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o..