Polymer Property : CTE, linear = 42.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 76.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E831
DuPont Bexloy® AXW504BK Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
CTE, linear 76.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E831
DuPont Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
CTE, linear 76.0 µm/m-°C

@Temperature 40.0 - 130 °C
42.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 2300 Phenolic, Granular, Compression Molded
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654..
CTE, linear <= 76.0 µm/m-°C

@Temperature 20.0 °C
<= 42.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Covestro Bayflex® 110-35 IMR Polyurethane Elastomeric RIM, 18% Mineral Filled, MDI-based 2-Component Liquid System
Calcium Silicate filled. 0.15 in. thickness. IMR=Internal Mold Release RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Ba..
CTE, linear 76.0 µm/m-°C
42.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® T7139 Glob Top Epoxy
Product Description: EPO-TEK® T7139 is a two component, electrically insulating, encapsulating epoxy designed for semiconductor glob top applications and package assembly.Advantages & Application N..
CTE, linear 76.0 µm/m-°C

@Temperature 20.0 °C
42.2 µin/in-°F

@Temperature 68.0 °F
Armstrong A-5/A Epoxy Adhesive
Information provided by Ellsworth Adhesives.
CTE, linear 76.0 - 170 µm/m-°C
42.2 - 94.4 µin/in-°F
Average value: 130 µm/m-°C Grade Count:20
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
CTE, linear 76.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E831
DuPont Bexloy® AXW502NC010 Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
CTE, linear 76.0 µm/m-°C

@Temperature 40.0 - 130 °C
42.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 1506 Polyester, Briquette, Injection Molded
PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop..
CTE, linear 76.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E831
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.