Polymer Property : CTE, linear = 400 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 400 µm/m-°C

@Temperature 20.0 °C
222 µin/in-°F

@Temperature 68.0 °F
Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer
Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlas..
CTE, linear 400 µm/m-°C

@Temperature 20.0 °C
222 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Kolon NOPLA® KE531HC PEN-PET Copolyester
NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac..
CTE, linear 400 µm/m-°C
222 µin/in-°F
Dow Corning 3-4150 DIELECTRIC GEL KIT
Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning