Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.62 µm/m-°C @Temperature 20.0 - 400 °C |
2.57 µin/in-°F @Temperature 68.0 - 752 °F |
|
Hogen HM1150 Tungsten-Based Metal Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
CTE, linear | 4.62 µm/m-°C @Temperature 20.0 - 400 °C |
2.57 µin/in-°F @Temperature 68.0 - 752 °F |
|
Mi-Tech Metals HD17.5 Tungsten-Based Metal Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2; ASTM B-777-07 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |