Thermal Properties Metric English Comments
CTE, linear 7.50 µm/m-°C
4.17 µin/in-°F
Plansee MoCu30 Molybdenum-Copper
Characteristics:High thermal conductivityLow thermal expansionLow densityApplications:Electronic components - passive cooling elementsAutomotive industry - carrier plates for IGBT modules in electri..
CTE, linear 7.50 µm/m-°C
4.17 µin/in-°F
Poco Graphite PYROGRAPH Ion Implant Grade Graphite
Pyrograph is pyrolytically infiltrated graphite. POCO's proprietary process infiltrates the base material to a minimum depth of 0.1 inch throughout the entire surface of the component. This process ..
CTE, linear 7.50 µm/m-°C
4.17 µin/in-°F
RSP Technology RSA-473 AH Aluminum Super Alloy
Alloy under development as of 2014. Used for Precision EquipmentFeatures: Low thermal expansion, low density, high stiffness, high thermal conductivityApplications: Electronic packaging, heat sinks..
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 °C
4.17 µin/in-°F

@Temperature 68.0 °F
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation
Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s..
CTE, linear 7.50 µm/m-°C
4.17 µin/in-°F
at Set Pt.
Ferro EG 2705 Glaze and Sealant Glass
Glass Type: Ca-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulat..
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 °C
4.17 µin/in-°F

@Temperature 68.0 °F
MarkeTech Aluminum Oxide Ceramic - Alumina 96%
Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture..
CTE, linear 7.50 µm/m-°C
4.17 µin/in-°F
Mateck Al2O3
Substrate bicrystals for superconductivity
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 °C
4.17 µin/in-°F

@Temperature 68.0 °F
GBC Grade 96 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 °C
4.17 µin/in-°F

@Temperature 68.0 °F
x-y direction
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite
Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate..
CTE, linear 7.50 µm/m-°C

@Temperature 25.0 - 600 °C
4.17 µin/in-°F

@Temperature 77.0 - 1110 °F
ICE Al2O3 94
Data provided by the manufacturer, International Ceramic Engineering.
CTE, linear 7.50 µm/m-°C

@Temperature 25.0 - 600 °C
4.17 µin/in-°F

@Temperature 77.0 - 1110 °F
ICE Al2O3 96
Data provided by the manufacturer, International Ceramic Engineering.
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 800 °C
4.17 µin/in-°F

@Temperature 68.0 - 1470 °F
Morgan Advanced Ceramics Sintoxâ„¢ FF Alumina
Alumina ceramic with a minimum Al2O3 content of 95.0% (typically 96%). This material is a high quality electrical insulator, with good mechanical properties, that is widely used for components in co..
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
Zircar Ceramics AL-30AAH Alumina Insulation
AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics.
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
Zircar Ceramics ZAL-15AA Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 °C
4.17 µin/in-°F

@Temperature 68.0 °F
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation
Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s..
CTE, linear 7.50 µm/m-°C

@Temperature 25.0 - 700 °C
4.17 µin/in-°F

@Temperature 77.0 - 1290 °F
Du-Co Ceramics S-470 Aluminum Silicate
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
CTE, linear 7.50 µm/m-°C

@Temperature 1000 °C
4.17 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SAL95 Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 7.50 µm/m-°C

@Temperature 1000 °C
4.17 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SAL99C Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
BNZ Materials BNZP-23B Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
BNZ Materials BNZP-26 Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
BNZ Materials BNZP-26A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
Anderman Ceramics EA96 Sintered Alumina, 96%
High strength alumina (96%) available pink or white. Available in many shapes and sizes.Information provided by Anderman Ceramics.
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
Zircar Ceramics AL-30AA Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
Zircar Ceramics ALCAA Alumina Insulation
ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics.
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.17 µin/in-°F

@Temperature 68.0 - 1830 °F
Zircar Ceramics ZAL-45AA Alumina Insulation
ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics.
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 600 °C
4.17 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C373
CeramTec 614/698 Alumina, 96%
614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink.
CTE, linear 7.50 µm/m-°C

@Temperature 20.0 - 100 °C
4.17 µin/in-°F

@Temperature 68.0 - 212 °F
DIN EN 821-1