Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 250 µm/m-°C | 139 µin/in-°F | ASTM E831 |
Parker Chomerics THERM-A-FORM T646 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
CTE, linear | 250 - 250 µm/m-°C @Temperature 70.0 - 150 °C |
139 - 139 µin/in-°F @Temperature 158 - 302 °F |
Average value: 250 µm/m-°C Grade Count:2 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear | 250 µm/m-°C | 139 µin/in-°F | Alpha 2 |
Lord Adhesives Thermosetâ„¢ MD-110 Conductive Adhesive LORD Thermosetâ„¢ MD-110 silver-filled conductive adhesive offers excellent electrical conductivity and room temperature stability. It is designed for use with automated dispensing, stamping and.. |
|||
CTE, linear | 250 µm/m-°C @Temperature 20.0 °C |
139 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV11 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
CTE, linear | 250 µm/m-°C @Temperature 20.0 °C |
139 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
CTE, linear | 250 µm/m-°C @Temperature 20.0 °C |
139 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV8111 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
CTE, linear | 250 µm/m-°C @Temperature 20.0 °C |
139 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV8112 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
CTE, linear | 250 µm/m-°C @Temperature 20.0 °C |
139 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV8112 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
CTE, linear | 250 µm/m-°C @Temperature 20.0 °C |
139 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
CTE, linear | 250 µm/m-°C @Temperature 20.0 °C |
139 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Micropol Isoplas P602 Crosslinkable Polyethylene Information provided by Micropol Limited |