Polymer Property : CTE, linear = 2.57 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 4.62 µm/m-°C

@Temperature 20.0 - 400 °C
2.57 µin/in-°F

@Temperature 68.0 - 752 °F
Hogen HM1150 Tungsten-Based Metal
Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE..
CTE, linear 4.62 µm/m-°C

@Temperature 20.0 - 400 °C
2.57 µin/in-°F

@Temperature 68.0 - 752 °F
Mi-Tech Metals HD17.5 Tungsten-Based Metal
Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2; ASTM B-777-07 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con..