Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 280 µm/m-°C | 156 µin/in-°F | Above Tg |
Tra-Con Tra-Duct 2960 Snap Cure Electrically Conductive Silver-Filled Epoxy TRA-DUCT 2960 is a one or two-part, specially refined and processed silver filled adhesive for high speed manufacturing. Recommended for the microelectronic, automotive computer and telecommunicatio.. |
|||
CTE, linear | 280 µm/m-°C | 156 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 868-3N1 Room Temperature Cure Adhesive TRA-BOND 868-3N1 room temperature cure adhesive provides strong bonds to difficult-to-bond metals, such as gold, silver, copper, brass, and solder.Information provided by Tra-Con Inc. |
|||
CTE, linear | 280 µm/m-°C | 156 µin/in-°F | Silicone Property; ASTM E 831 |
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d.. |