Polymer Property : CTE, linear = 144 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 144 µm/m-°C

@Temperature -40.0 - 149 °C
80.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® HPV UHMW-PE (ASTM Product Data Sheet)
CTE, linear 144 µm/m-°C

@Temperature 20.0 °C
80.0 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ CC191-HE PTFE, 25% Carbon/Graphite Filled  (discontinued **)
Product Form: Black, non-pelletized powder. Applications include bearings, bushings.Data provided by Dyneon.
CTE, linear 144 µm/m-°C
80.0 µin/in-°F
Saint-Gobain Rulon® II Bearing/Seal PTFE
An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al..
CTE, linear 144 µm/m-°C

@Temperature 50.0 - 200 °C
80.0 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT 8001 Polytetrafluoroethylene (PTFE) + Polyimide, 20% (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear 144 µm/m-°C
80.0 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® 430 Epoxy
Product Description: A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding ..
CTE, linear 144 - 180 µm/m-°C

@Temperature 25.6 - 204 °C
80.0 - 100 µin/in-°F

@Temperature 78.0 - 400 °F
ASTM D696
Technetics Group Texolon™ 8534 PTFE  (Unverified Data**)
PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectric ConstantHigh Volume and Surface ResistivityFlame ResistanceApp..
CTE, linear 144 µm/m-°C

@Temperature 24.0 - 149 °C
80.0 µin/in-°F

@Temperature 75.2 - 300 °F
ASTM E831-93
Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..