Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 19.8 - 139 µm/m-°C | 11.0 - 77.2 µin/in-°F | Average value: 72.2 µm/m-°C Grade Count:46 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
CTE, linear | 119 - 139 µm/m-°C @Temperature 20.0 °C |
66.0 - 77.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® PVDF Fluoropolymer Film Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from.. |