Thermal Properties Metric English Comments
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-101 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-120 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-130 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-21 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion ..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-30 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-40 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-20 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,..
CTE, linear 83.0 - 105 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 - 58.3 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON NP-3000 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi..
CTE, linear 95.0 - 105 µm/m-°C

@Temperature 20.0 °C
52.8 - 58.3 µin/in-°F

@Temperature 68.0 °F
Abatron AboCast/AboCure 8109-10
2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro..