Polymer Property : CTE, linear = 0.0522 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 0.0940 µm/m-°C

@Temperature 20.0 °C
0.0522 µin/in-°F

@Temperature 68.0 °F
ASTM E831
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy
Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an..