Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | <= 100 mm/min | <= 3.94 in/min | 1.6mm; GM9070P |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Flame Spread | <= 100 mm/min | <= 3.94 in/min | FMVSS - 302 flame propagation rate; DIN 75200 |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) at 50% RH Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Flame Spread | <= 100 mm/min | <= 3.94 in/min | FMVSS - 302 flame propagation rate; DIN 75200 |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) at 50% RH Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
Flame Spread | <= 100 mm/min | <= 3.94 in/min | DIN 75200 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Flame Spread | <= 100 mm/min | <= 3.94 in/min | DIN 75200 |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
Flame Spread | <= 100 mm/min | <= 3.94 in/min | DIN 75200 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Flame Spread | <= 100 mm/min | <= 3.94 in/min | DIN 75200 |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Flame Spread | <= 100 mm/min | <= 3.94 in/min | DIN 75200 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Flame Spread | <= 100 mm/min | <= 3.94 in/min | DIN 75200 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |