Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 25.0 mm/min @Thickness 1.00 mm |
0.984 in/min @Thickness 0.0394 in |
FMVSS 302 |
SABIC Innovative Plastics Cycolac® G320 ABS (Europe-Africa-Middle East) CYCOLAC G320 is a super high impact resistant ABS grade. It combines impact resistance with high stiffness, good temperature resistance and processability. It has a good fit in automotive interiors .. |
|||
Flame Spread | 25.0 mm/min @Thickness 1.00 mm |
0.984 in/min @Thickness 0.0394 in |
FMVSS 302 |
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East) CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments.. |
|||
Flame Spread | 25.0 mm/min @Thickness 1.00 mm |
0.984 in/min @Thickness 0.0394 in |
FMVSS 302 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Flame Spread | 25.0 mm/min @Thickness 3.17 mm |
0.984 in/min @Thickness 0.125 in |
FH3 |
LG Chemical 81HF SAN Resin High flow, Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include food receptacles, disposable li.. |
|||
Flame Spread | 25.0 mm/min @Thickness 3.17 mm |
0.984 in/min @Thickness 0.125 in |
FH3 |
LG Chemical 95HC SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring.. |
|||
Flame Spread | 25.0 mm/min | 0.984 in/min | BH3; VDE 0304T3 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |