Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Decomposition Temperature = 388 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 388 °C
730 °F
Hybrid Plastics POSS® MA0705 MethacrylCyclopentyl-POSS®
POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS®..
Decomposition Temperature 388 °C
730 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H44 Gold-Filled, Electrically Conductive Epoxy
Product Description: EPO-TEK® H44 is a single component, gold-filled, electrically conductive epoxy adhesive designed for hybrid microelectronic packaging.Advantages & Application Notes: High visco..
Copyright © lookpolymers.com All Rights Reserved