Thermal Properties Metric English Comments
Flash Point 97.0 °C
207 °F
PMCC
Dow Hydroxypropyl Acrylate
Hydroxypropyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow
Flash Point 97.0 °C
207 °F
Closed cup
Dow Corning 5330 Fluid
A polysiloxane polyether copolymer for use in hair care applications.Information provided by Dow Corning