Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 90.0 °C | 194 °F | Seta |
LyondellBasell NMP N-methyl-2-pyrrolidone Available in electronic grade.Information provided by Lyondell. |
|||
Flash Point | 90.0 °C | 194 °F | ASTM D93 |
ExxonMobil Mobil Aero HF Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Flash Point | >= 90.0 °C | >= 194 °F | closed cup |
Dow Corning SYL-OFF® 7682-000 CROSSLINKER Syl-Off® 7682-000 Crosslinker is a 100% active solids silicone crosslinker. Recommended where optimum anchorage to substrate and good cure are required. Compatible with Syl-Off® 7680 Series Coatin.. |
|||
Flash Point | >= 90.0 °C | >= 194 °F | Closed cup |
Dow Corning SYL-OFF® PMCP7682-000 Crosslinker Syl-Off® 7682-000 Crosslinker is a 100% active solids silicone crosslinker. Recommended where optimum anchorage to substrate and good cure are required. Compatible with Syl-Off® 7680 Series Coatin.. |
|||
Flash Point | 90.0 °C | 194 °F | Open cup |
Dow Corning EL-8051 IN Silicone Organic Elastomer Blend Combine the feel of silicone elastomer gels with a wider range of organic ingredients and actives. Our silicone organic elastomer blends can give you the innovative freedom to create color cosmetics.. |
|||
Flash Point | 90.0 °C | 194 °F | |
BASF DiethylenetriaminE Formula: C4H13N3CAS: 111-40-0Description: Diethylenetriamine is a colorless to yellow liquid with an amine-like odor.Synonyms: DETA, Bis(2-aminoethyl)amine, 1,4,7-Triazaheptane, 1,5-Diamino-3-azapen.. |
|||
Flash Point | 90.0 °C | 194 °F | |
BASF Lupragen® N 201 TEDA in DPG Formula: C6H12N2CAS: 280-57-9Description: Lupragen® N 201 is a solution in dipropylene glycol and is a colorless to yellow liquid, with a faint specific odor characteristic with this product. It i.. |
|||
Flash Point | 90.0 °C | 194 °F | |
BASF Lupragen® N 107 Dimethylaminoethoxyethanol Formula: C6H15NO2CAS: 1704-62-7Description: Dimethylaminoethoxyethanol is a colorless to yellowish liquid, with an amine-like odor. It is miscible with water.Synonyms: DMEE, (N,N-Dimethylaminoethox.. |
|||
Flash Point | 90.0 °C | 194 °F | ASTM D93 |
ExxonMobil Mobil Aero HF Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |