Polymer Property : Flash Point = 77.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 77.0 °C
171 °F
Lord Adhesives 310 High Strength SMC, FRP and General Purpose Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Flash Point 77.0 °C
171 °F
Lord Adhesives 312 General Purpose, Low Viscosity Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Flash Point 77.0 °C
171 °F
Closed cup
Dow Corning 9011 Silicone Elastomer Blend
A dispersion of high molecular weight silicone elastomer substituted with polyether in cyclopentasiloxane for use in skincare, suncare, color cosmetics, and antiperspirant / deodorant applications.I..
Flash Point 77.0 °C
171 °F
Closed cup
Dow Corning ST Cyclomethicone 5-NF
Volatile silicone, decamethylcyclopentasiloxane (Cyclomethicone NF) for use in a wide range of skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning
Flash Point 77.0 °C
171 °F
Closed Cup
Dow Corning XIAMETER® PMCPPMX-0245 Cyclopentasiloxane
Is chemically equivalent to DOW CORNING® 245 FLUID. This product a volatile, low viscosity cyclopentasiloxane fluid for use in skincare, suncare, color cosmetics, hair care, and antiperspirant / de..
Flash Point 77.0 °C
171 °F
Closed Cup
Dow Corning XIAMETER® PMCPPMX-0345 Cyclosiloxane Blend
Is chemically equivalent to DOW CORNING® 345 FLUID. A blend of polydimethylcyclosiloxanes composed mainly of cyclopentasiloxane and cyclohexasiloxane for use in skincare, suncare, color cosmetics, ..
Flash Point 77.0 °C
171 °F
Closed cup
Dow Corning 5200 Formulation Aid
An alkylmethyl siloxane copolyol designed to prepare stable water-in-oil emulsions.Information provided by Dow Corning
Flash Point >= 77.0 °C
>= 171 °F
Closed cup
Dow Corning 5225C Formulation Aid
A 10% dispersion of high molecular weight silicone polyether in cyclopentasiloxane fluid for use in skincare, suncare, hair care, color cosmetic, and antiperspirant / deodorant applications. INCI Na..
Flash Point 77.0 °C
171 °F
Closed cup
Dow Corning 3-3009 Cosmetic Wax
An emulsifier base comprised of a silicone fluid blend and emulsifier for use in skincare, suncare, shower gels, color cosmetics, and antiperspirant / deodorant applications.Information provided by ..