Polymer Property : Flash Point = 76.6 °C
Polymer Property :
Flash Point =
76.6 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Flash Point
76.6
°C
170
°F
Closed cup
Dow Corning 5329 Modifier