Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G50S FFKM White Perfluoroelastomer Perlast® G50S FFKM is a White Perfluoroelastomer 50-55 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and extr.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G60A Perfluoroelastomer A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Suitable for app.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G60S FFKM White Perfluoroelastomer Perlast ® G60S FFKM is a White Perfluoroelastomer 56-65 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and ext.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G60T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: This grade is particularly suited to static ap.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G70A Perfluoroelastomer A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applicat.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer Special white compound with wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Recommended f.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G70R Red Perfluoroelastomer Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G80A Perfluoroelastomer A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Do not use any P.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G80H Perfluoroelastomer Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G80S FFKM White Perfluoroelastomer Perlast ® G80S FFKM is a White Perfluoroelastomer 76-85 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and ext.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G80X Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G81H Perfluoroelastomer Special, pure white compound with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. .. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G81T Perfluoroelastomer A special black perfluoroelastomer compound with PTFE blended for improved mechanical performance. Excellent steam resistance and mechanical properties. Extremely low outgassing properties. Applica.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G90A Perfluoroelastomer A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applicat.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G90S White Perfluoroelastomer Perlast ® G90S is a White Perfluoroelastomer 86-95 °IRHD with excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and formulated .. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G92A Perfluoroelastomer An electrically conductive black perfluoroelastomer with excellent chemical and steam resistance.Applications: Specially formulated for applications requiring special electrical properties. Origina.. |
|||
Flash Point | >= 400 °C | >= 752 °F | |
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer Special, white compound, with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. Appl.. |
|||
Flash Point | 400 °C | 752 °F | |
LG Chemical EM500 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Flash Point | 400 °C | 752 °F | |
LG Chemical EM500A Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Flash Point | 400 °C | 752 °F | |
LG Chemical IM810 Acrylic impact modifier Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro.. |
|||
Flash Point | 400 °C | 752 °F | |
LG Chemical MB802 Transparent impact modifier Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra.. |
|||
Flash Point | 400 °C | 752 °F | |
LG Chemical MB838A Opaque impact modifier Description: MBS type opaque impact modifiers from LG Chem are appropriate for improving impact strength all the PVC products of rigid and semi-rigid opaque PVC, and have differentiated characterist.. |
|||
Flash Point | 400 °C | 752 °F | |
LG Chemical MB872 Transparent impact modifier Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra.. |
|||
Flash Point | 400 °C | 752 °F | |
LG Chemical MB885 Transparent impact modifier Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra.. |
|||
Flash Point | 400 °C | 752 °F | |
LG Chemical IM812 Acrylic impact modifier Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro.. |