Thermal Properties Metric English Comments
Flash Point 20.6 °C
69.1 °F
9924V; Setaflash, Closed Cup; ASTM D3278-82
Lord Adhesives Aeroglaze® 9924V Wash Primer
Aeroglaze® 9924V wash primer was designed for priming metal surfaces. It is particularly useful for priming non-ferrous substrates such as aluminum and galvanized steel.All information provided b..