Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 48.9 °C | 120 °F | CC |
LG Chemical Butyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |