Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 9.00 °C | 48.2 °F | Seta |
LyondellBasell Ethanol, 200 Proof Information provided by Lyondell. |
|||
Flash Point | 9.00 °C | 48.2 °F | CC |
LG Chemical Ethyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |
|||
Flash Point | 9.00 °C | 48.2 °F | |
Lord Adhesives 513 Fast Cure, Non-Sagging Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Flash Point | 9.00 °C | 48.2 °F | Seta |
Lord Adhesives Chemlok® 607 Adhesive LORD Chemlok® 607 adhesive is a clear, colorless adhesive used to bond unvulcanized silicone rubber to various substrates such as metals, glass, plastics and textiles.Chemlok 607 adhesive also bo.. |
|||
Flash Point | 9.00 °C | 48.2 °F | closed cup |
Dow Corning S 2260 PRIME COAT Information provided by Dow Corning |
|||
Flash Point | 9.00 °C | 48.2 °F | closed cup |
Dow Corning Z-6079 SILANE DOW CORNING Z6079 Silane is useful in protecting OH and SH functionality of complex molecules, permitting other sites to be selectively reacted.Information provided by Dow Corning |