Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 460 °C | 860 °F | ASTM D 1929 |
Covestro Makrolon® 1881 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp.. |
|||
Flash Point | 460 °C | 860 °F | ASTM D 1929 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Flash Point | 460 °C | 860 °F | ASTM D 1929 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Flash Point | 460 °C | 860 °F | ASTM D 1929 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Flash Point | 460 °C | 860 °F | ASTM D 1929 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Flash Point | 460 °C | 860 °F | ASTM D 1929 |
Covestro Makrolon® 6165 X Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Low.. |
|||
Flash Point | 460 °C | 860 °F | ASTM D 1929 |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |