Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 7.22 °C | >= 45.0 °F | |
Parker Chomerics CHO-BOND 586 Conductive Epoxy Information provided by Chomerics |
|||
Flash Point | >= 7.22 °C | >= 45.0 °F | |
Parker Chomerics CHO-SHIELD® 576 Part B Coating Catalyst Information provided by Chomerics |
|||
Flash Point | 7.22 - 150 °C | 45.0 - 302 °F | Average value: 105 °C Grade Count:7 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Flash Point | 7.22 °C | 45.0 °F | ASTM D56 |
ExxonMobil Exxsol™ DSP100/160 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Flash Point | 7.22 °C | 45.0 °F | ASTM D56 |
ExxonMobil Isopar™ E Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Asia .. |