Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 430 °C | 806 °F | ASTM D92 |
ChevronTexaco 128 Refined Wax FeaturesChevron Refined Waxes are fully refined, food grade waxes meeting the highest purity standards. Derived from petroleum using a solvent refining process, Chevron Refined Waxes are comprised .. |
|||
Flash Point | 430 °C | 806 °F | Average value: 430 °C Grade Count:4 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |