Polymer Property : Flash Point = 400 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G50S FFKM White Perfluoroelastomer
Perlast® G50S FFKM is a White Perfluoroelastomer 50-55 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and extr..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G60A Perfluoroelastomer
A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Suitable for app..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer
Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G60S FFKM White Perfluoroelastomer
Perlast ® G60S FFKM is a White Perfluoroelastomer 56-65 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and ext..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G60T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: This grade is particularly suited to static ap..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G70A Perfluoroelastomer
A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applicat..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer
Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer
Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer
Special white compound with wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Recommended f..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G70R Red Perfluoroelastomer
Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G80A Perfluoroelastomer
A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Do not use any P..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G80H Perfluoroelastomer
Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G80S FFKM White Perfluoroelastomer
Perlast ® G80S FFKM is a White Perfluoroelastomer 76-85 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and ext..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G80X Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G81H Perfluoroelastomer
Special, pure white compound with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. ..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G81T Perfluoroelastomer
A special black perfluoroelastomer compound with PTFE blended for improved mechanical performance. Excellent steam resistance and mechanical properties. Extremely low outgassing properties. Applica..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G90A Perfluoroelastomer
A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applicat..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G90S White Perfluoroelastomer
Perlast ® G90S is a White Perfluoroelastomer 86-95 °IRHD with excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and formulated ..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G92A Perfluoroelastomer
An electrically conductive black perfluoroelastomer with excellent chemical and steam resistance.Applications: Specially formulated for applications requiring special electrical properties. Origina..
Flash Point >= 400 °C
>= 752 °F
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer
Special, white compound, with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. Appl..
Flash Point 400 °C
752 °F
LG Chemical EM500 Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Flash Point 400 °C
752 °F
LG Chemical EM500A Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Flash Point 400 °C
752 °F
LG Chemical IM810 Acrylic impact modifier
Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro..
Flash Point 400 °C
752 °F
LG Chemical MB802 Transparent impact modifier
Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra..
Flash Point 400 °C
752 °F
LG Chemical MB838A Opaque impact modifier
Description: MBS type opaque impact modifiers from LG Chem are appropriate for improving impact strength all the PVC products of rigid and semi-rigid opaque PVC, and have differentiated characterist..
Flash Point 400 °C
752 °F
LG Chemical MB872 Transparent impact modifier
Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra..
Flash Point 400 °C
752 °F
LG Chemical MB885 Transparent impact modifier
Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra..
Flash Point 400 °C
752 °F
LG Chemical IM812 Acrylic impact modifier
Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro..