Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 32.5 °C | 90.5 °F | |
BASF Tripropylamine Formula: C9H21NCAS: 102-69-2Description: Tripropylamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water. Synonyms: Propyldi-n-propylamine, Tri-n-propylamine, N,N-Di.. |