Thermal Properties Metric English Comments
Flash Point >= 134 °C
>= 273 °F
Parker Chomerics CHO-SHIELD® 4937 Part B Barrier Coating Component
Information provided by Chomerics
Flash Point 134 °C
273 °F
Open Cup
Dow Corning XIAMETER® PMCPPMX-200 5CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 5CS. 100% active, 5 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Flash Point 134 °C
273 °F
BASF 1,4-Butanediol (BDO)
Formula: C4H10N2CAS: 110-63-4Description: 1,4-Butanediol (BDO) is a colorless, odorless liquid. It is miscible in all proportions with water and soluble with organic solvent.Synonyms: Butane-1,4-di..