Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flash Point = 26.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 26.0 °C
78.8 °F
ASTM D3278, Seta Flash, Closed Cup
Lord Adhesives Chemglaze® V021 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Flash Point 26.0 °C
78.8 °F
closed cup
Dow Corning 7355 ADHESIVE
Dow Corning® 7355 Adhesive is a dispersion of polydimethylsiloxane gum and resin; is blendable with a variety of other dimethyl type silicone PSA's. Provides excellent balance of adhesion and tack,..
Flash Point 26.0 °C
78.8 °F
closed cup
Dow Corning SYL-OFF® 23-30% COATING
Syl-Off® 23 Paper Coating 30 Percent is a 30% active solids dispersion of silanol functional silicone polymers and multifunctional crosslinkers in xylene.Information provided by Dow Corning
Flash Point >= 26.0 °C
>= 78.8 °F
closed cup
Dow Corning SYL-OFF® 294 COATING
Syl-Off® 294 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 40 percent solids dispersion of a blend of reactive silox..
Flash Point 26.0 °C
78.8 °F
BASF N,N-Dimethylisopropanolamine
Formula: C5H13NOCAS: 108-16-7Description: Dimethylisopropanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: Dimethylisopropanolamine, 1-Dimethylami..
Flash Point 26.0 °C
78.8 °F
BASF Propyl Chloroformate
Formula: C4H6ClO2CAS: 109-61-5Description: Propyl Chloroformate is a colorless to yellow liquid, with a pungent odor. It reacts with water and spontaneous decomposes.Synonyms: Chloroformic acid pro..
Flash Point 26.0 °C
78.8 °F
Oceanchem Group n-Propyl Bromide (NPB)
Molecular Formula: C3H7BrCas No.: 106-94-5Applications: Solvent for industrial cleaning, organic synthesis, pharmaceutical intermediate.Information Provided by Oceanchem Group