Polymer Property : Flash Point = 255 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 124 °C
255 °F
Pensky-Martens
LyondellBasell TPNB Tripropylene glycol normal butyl ether
Information provided by Lyondell.
Flash Point 124 °C
255 °F
closed cup
Dow Corning SYL-OFF® 7040 COATING
Syl-Off® 7040 Coating is a 100% active solids coating containing a low viscosity hexenyl endblocked and pendant functional silicone polymer. Recommended for fast cure and stable release against agg..
Flash Point 124 °C
255 °F
Closed cup
Dow Corning SYL-OFF® PMCP7040 Coating
Syl-Off® 7040 Coating is a 100% active solids coating containing a low viscosity hexenyl endblocked and pendant functional silicone polymer. Recommended for fast cure and stable release against agg..