Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flash Point = 250 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 121 °C
250 °F
ASTM D56
Humiseal 1C51 Silicone Conformal Coating
Humiseal 1C51 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605..
Flash Point 121 °C
250 °F
ASTM D56
Humiseal 1C55 Silicone Conformal Coating
Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock ..
Flash Point 121 °C
250 °F
Pensky-Martens
LyondellBasell TPM Tripropylene glycol methyl ether
Information provided by Lyondell.
Flash Point >= 121 °C
>= 250 °F
Closed Cup
Solvay STANNINE® LTP Surfactant
Description: Dispersant with binding properties.Identification: BLEND OF SUBSTITUTED THIOUREA AND SURFACTANTSSolubility: Soluble in acid solutions. Insoluble in water or neutral solutions.Available ..
Flash Point 121 °C
250 °F
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy
Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable ..
Flash Point 121 °C
250 °F
closed cup
Dow Corning SYL-OFF® 7671 COATING
Syl-Off® 7671 Coating is a 100% active solids, pre-catalysed, coating containing a low viscosity hexenyl endblocked only functional silicone polymer. Provides fast cure and stable premium release p..
Flash Point 121 °C
250 °F
Closed cup
Dow Corning SYL-OFF® PMCP7671 Coating
Syl-Off® 7671 Coating is a 100% active solids, pre-catalysed, coating containing a low viscosity hexenyl endblocked only functional silicone polymer. Provides fast cure and stable premium release p..
Flash Point 121 °C
250 °F
open cup
Dow Corning SZ-1180 Silicone Surfactant
Dow Corning® SZ-1180 Additive is a non-hydrolyzable silicone surfactant recommended for production of flexible slab stock PU foam.Information provided by Dow Corning
Flash Point >= 121 °C
>= 250 °F
ConocoPhillips Gear Shield NC Open Gear Lubricant
Description: Conoco Gear Shield NC is a black, viscous fluid designed to lubricate open gears. Gear Shield NC contains neither chlorinated solvents nor lead compounds. Gear Shield NC is designed to ..
Flash Point 121 °C
250 °F
ASTM D-92
ConocoPhillips Hydroclear® 2 Ultra-Clean Spindle Oil
Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties o..
Flash Point 121 °C
250 °F
BASF DEHA DI-2-Ethylhexylamine
Formula: C16H35NCAS: 106-20-7Description: DEHA is a colorless to yellow liquid, with an amine-like odor. It is also miscible with water in all proportions.Synonyms: DEHA, Di-(2-Ethylhexyl)-amineAppl..
Flash Point >= 121 °C
>= 250 °F
Dow Corning 3099 HVIC COMPOUND
Dow Corning 3099 is a grease-like silicone coating especially formulated to give electrical insulators long-term resistance to water filming and flashover.Features: Protecting electrical insulators...
Copyright © lookpolymers.com All Rights Reserved