Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 211 °C | 412 °F | COC |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 30 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |
|||
Flash Point | 211 °C | 412 °F | Closed Cup |
Dow Corning XIAMETER® PMCPPMX-200 10CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 10CS. 100% active, 10 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |