Polymer Property : Flash Point = 19.3 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 19.3 °C
66.7 °F
Setaflash, Closed Cup; ASTM D3278-82
Lord Adhesives Aeroglaze® Z307 Absorptive Conductive Polyurethane
Aeroglaze® Z307 black absorptive conductive polyurethane coating is primarily for application to substrates used on spacecraft. These applications include those where coatings must exhibit low ou..
Flash Point 19.3 °C
66.7 °F
Setaflash, Closed Cup; ASTM D3278-82
Lord Adhesives Aeroglaze® A276 Reflective Polyurethane
Aeroglaze® A276 reflective polyurethane gives a hard, flexible, colorfast, non-chalking surface that is resistant to most acids, alkaline detergents, lubricants, and chemicals.All information provi..