Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 82.2 °C | 180 °F | |
Palm Labs Adhesives TURBO-LOCK SERIES 20 Anaerobic Thread Locking Compound TURBO-LOCK SERIES 20 is a fast curing, BLUE, low strength, thread locker for bonding and sealing small plastic fasteners. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbon.. |
|||
Flash Point | 82.2 °C | 180 °F | Method A; ASTM D93 |
ExxonMobil Exxsol™ D80 Dearomatized Fluid Availability: Africa & Middle East, Asia Pacific, Europe, Central America, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Flash Point | 82.2 °C | 180 °F | Method A; ASTM D93 |
ExxonMobil Isopar™ M (EU) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and Eu.. |
|||
Flash Point | 82.0 °C | 180 °F | Setaflash closed cup |
3M Novec™ FC-4430 Fluorosurfactant 3M™ Novec™ Fluorosurfactant FC-4430 is a non-ionic polymeric fluorochemical surfactant belonging to a class of coating additives which provide low surface tensions in coating systems best served b.. |
|||
Flash Point | 82.0 °C | 180 °F | Setaflash closed cup |
3M Novec™ FC-4432 Fluorosurfactant 3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga.. |