Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 63.0 °C | 145 °F | closed cup |
Dow Corning Z-6341 SILANE Dow Corning® Z-6341 Silane is high purity, undiluted N-octyltriethoxy-silane. When diluted with an appro-priate solvent, it can be used in the formulation of water repellent prod-ucts. Upon proper .. |
|||
Flash Point | 62.8 °C | 145 °F | ASTM D56 |
ExxonMobil Varsol™ DX 140 Naphtha Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Flash Point | 63.0 °C | 145 °F | closed cup |
Dow Corning 19 ADDITIVE DOW CORNING 19 Additive is a modified silicone, designed primarily to provide levelling, slip and mar resistance in water and solvent borne paints, inks and coatings. This additive also improves ant.. |
|||
Flash Point | >= 63.0 °C | >= 145 °F | closed cup |
Dow Corning 190 Fluid Dow Corning® 190 Fluid is a silicone glycol copolymer.Information provided by Dow Corning |