Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flash Point = 142 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point >= 61.0 °C
>= 142 °F
Solvay GERONOL® FF/4-E Surfactant
Description: Multipurpose emulsifier for agrochemical formulations. Used in pair with Geronol FF/6-C or MS-C.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most pola..
Flash Point >= 61.0 °C
>= 142 °F
Solvay GERONOL® FF/6-E Surfactant
Description: Multipurpose emulsifier for EC, to use in pair with Geronol FF/4 or Rhodacal 70/B.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most polar and aromatic..
Flash Point >= 61.0 °C
>= 142 °F
Solvay GERONOL® TE 300 Surfactant
Description: Emulsifier for agrochemical formulations.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most polar and aromatic solventsAvailable in: Asia Pacific, Euro..
Flash Point >= 61.0 °C
>= 142 °F
Solvay RHODACAL® 60/BE Surfactant
Description Anionic, high flash point, linear Calcium dodecylbenzene sulfonate, 60% active , useful in emulsifier blends where high flash point is required.Identification: LINEAR DODECYLBENZENE SULP..
Flash Point >= 61.0 °C
>= 142 °F
Closed cup
Dow Corning Q2-5247 Fluid
Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning
Flash Point 61.0 °C
142 °F
closed cup
Dow Corning Z-6376 SILANE
Chloropropyltriethoxysilane - Used to pretreat or be added to the resin for integral treatment. Improves chemical bonding of resins to inorganic materials.Information provided by Dow Corning
Flash Point 61.1 °C
142 °F
Method A; ASTM D93
ExxonMobil Isopar™ J Isoparaffin Fluid
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and Eu..
Flash Point >= 61.1 °C
>= 142 °F
Closed cup
Dow Corning 2-2647 Performance Modifier
Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning
Flash Point >= 61.0 °C
>= 142 °F
Solvay RHODISOLV® GREEN 21 Solvent
Identification: BLEND OF SOLVENTSAvailable in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Insoluble in water. Soluble in most polar and aromatic solvents. Applications: Solvent..
Flash Point >= 61.0 °C
>= 142 °F
Solvay RHODISOLV® GREEN 25 Solvent
Identification: BLEND OF SOLVENTSAvailable in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Insoluble in water. Soluble in most polar and aromatic solvents. Applications: Solvent..