Polymer Property : Flash Point = -18.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point -18.0 °C
-0.400 °F
ASTM D93, DIN 51 755
Chesterton 294 CSD Industrial Degreaser
Description: Chesterton® 294 CSD is a fast acting, industrial degreaser for critical equipment. It contains no chlorinate, aromatic or solvents of questionable toxicity. Designed to quickly penetra..
Flash Point -18.0 °C
-0.400 °F
3M Scotch-Seal™ 2084 Metal Sealant
Features: 3M™ Scotch-Seal™ Metal Sealant 2084 is a one-part aluminum colored sealant which air dries to a tough, flexible film that resists water, oils and fuel. Retains sealing properties after e..
Flash Point -18.0 °C
-0.400 °F
TCC
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives
Features: It is a low viscosity grade for spray application.Fast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (Ma..
Flash Point -18.0 °C
-0.400 °F
TCC
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive
Features: Low viscosity grade for spray applicationFast dryingProvides strong, flexible bondsResists weathering, water, fuels, oil and plasticizersBonds vinyl extrusions and sheeting (May stain ligh..
Flash Point -18.0 °C
-0.400 °F
CC
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..
Flash Point -18.0 °C
-0.400 °F
CC
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..
Flash Point -18.0 °C
-0.400 °F
CC
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..
Flash Point -18.0 °C
-0.400 °F
TCC
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives
Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a..
Flash Point -18.0 °C
-0.400 °F
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..