Polymer Property : Flash Point = -12.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point -12.0 - 253 °C
10.4 - 487 °F
Average value: 57.1 °C Grade Count:19
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
Flash Point -12.0 °C
10.4 °F
Pensky-Martin Closed Cup
Momentive Performance Materials SS4004P Silicone Primer for use with RTV Silicone Adhesive Sealants, Pink
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion..
Flash Point -12.0 °C
10.4 °F
Pensky-Martin Closed Cup
Momentive Performance Materials SS4044P Silicone Primer for use with RTV Silicone Adhesive Sealants, Light Yellow
SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants.  GE Silicones one-component products offer primerless adhesion..
Flash Point -12.0 °C
10.4 °F
Tag open cup
Momentive Performance Materials SS4171P Addition Cure Silicone Rubber Molding Compounds
SS4171P model sealer is used to help minimize cure inhibition of addition curing silicone rubber moldmaking material. Properly applied, the model sealer will help to prevent substrates such as sulf..
Flash Point -12.0 °C
10.4 °F
3M 2262T Adhesion Promoter
3M™ Adhesion Promoter 2262AT is a ready-to-use, pre-diluted (10 parts Acetone/1 part 2262) version of 3M™ Scotch-Grip™ Plastic Adhesive 2262. It is a liquid promoter intended for most flexible an..
Flash Point -12.0 °C
10.4 °F
3M 2262T Adhesion Promoter
3M Adhesion Promoter 2262T is a ready-to-use, pre-diluted (10 MEK/1 part 2262) version of 3M Scotch-Grip Plastic Adhesive 2262. It is a liquid primer intended for most flexible and rigid PVC compoun..