Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 400 °C | 752 °F | |
LG Chemical DINP Plasticizer Features: LG DINP is used cable and tarpaulin because it can reduce gas generation during operation due to low volatile compared to DOP.Application: Synthetic leather, sheet, power cableInformation .. |
|||
Boiling Point | 400 - 416 °C | 752 - 781 °F | |
LG Chemical LGflex GL100 Plasticizer Features: Excellent Heat Loss and Non-endocrine disrupter Application: PVC Power Cable, SheetsInformation provided by LG Chemical |
|||
Boiling Point | 400 °C | 752 °F | |
LG Chemical LGflex GL300 Plasticizer Features: Excellent Viscosity, Heat Stability and Non-endocrine disrupterApplication: PVC Calenderings/Leathers, Sheets, Gloves, HoseInformation provided by LG Chemical |