Thermal Properties Metric English Comments
Boiling Point 206 °C
403 °F
Initial; ASTM D86
ExxonMobil Isopar™ M (EU) Isoparaffin Fluid
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and Eu..
Boiling Point 206 °C
403 °F
BASF DiethylenetriaminE
Formula: C4H13N3CAS: 111-40-0Description: Diethylenetriamine is a colorless to yellow liquid with an amine-like odor.Synonyms: DETA, Bis(2-aminoethyl)amine, 1,4,7-Triazaheptane, 1,5-Diamino-3-azapen..
Boiling Point 206 - 208 °C
403 - 406 °F
BASF N-Methylacetamide
Formula: C2H7NOCAS: 79-16-3Description: N-Methylacetamide is a colorless solid with a faint amine-like odor. It is fairly soluble with water and other organic solvents. Synonyms: Mono-N-methylaceta..