Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 33.0 °C @Pressure 0.000667 MPa |
91.4 °F @Pressure 0.0967 psi |
|
LG Chemical LGflex TINTM Plasticizer Features: New plasticizer is required high heat-resistance and weatherability because it is strengthen of UL standard. LGflex TINTM is excellent ins higher heat-resistance and weatherability than co.. |