Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 264 °C | 507 °F | |
Dow Corning Z-6094 SILANE Aminoethylaminopropyltrimethoxysilane - H2NC2H4NHC3H6-Si(OCH3)3. High purity version of Z-6020, coupling agent.Information provided by Dow Corning |
|||
Boiling Point | 264 °C | 507 °F | |
BASF N-Butyldiethanolamine Formula: C8H19NO2CAS: 102-79-4Description: N-Butyldiethanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible with water in all proportions.Synonyms: BDEA, N-Butyldiethan.. |