Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 172 °C | 342 °F | |
LG Chemical DCPD Structure & Characteristics: Dimer of cyclopentadiene. Purified after Isolating from pyrolysis oil evolved during NCC pyrolysis processUses: Used during manufacturing of unsaturated polyester resin .. |
|||
Boiling Point | 172 °C | 342 °F | |
Dow Corning XIAMETER® PMCPPMX-0244 Cyclotetrasiloxane Is chemically equivalent to DOW CORNING® 244 FLUID. This product is a volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension and evaporates completely at room.. |