Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 139 °C | 282 °F | |
BASF Isobutyl Acrylate Formula: C7H12O2CAS: 106-63-8Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Isobutyl acrylate forms homopolymers and copolymers. Copol.. |