Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 79.0 °C | 174 °F | ASTM D1525 |
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo.. |