Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 185 °C | 365 °F | |
Valley Adhesives EM-600 High Temperature Application Glue Stick Valley Adhesives EM-600 High Temperature Application Glue StickBonds many woods and wood composites; Excellent for woodworking and cabinetry. |
|||
Softening Point | 185 °C | 365 °F | |